| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics Lexan® 500 PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Density | 1.245 g/cc | 0.04498 lb/in³ | ASTM D792 |
| Water Absorption | 0.12 % @Time 86400 sec |
0.12 % @Time 24.0 hour |
ASTM D570 |
| Moisture Absorption at Equilibrium | 0.31 % | 0.31 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 85 | 85 | ASTM D785 |
| Hardness, Rockwell R | 124 | 124 | ASTM D785 |
| Tensile Strength at Break | 55.0 MPa | 7980 psi | Type I, 5 mm/min; ASTM D638 |
| Tensile Strength, Yield | 66.0 MPa | 9570 psi | Type I, 5 mm/min; ASTM D638 |
| Elongation at Break | 15 % | 15 % | Type I, 5 mm/min; ASTM D638 |
| Elongation at Yield | 8.0 % | 8.0 % | Type I, 5 mm/min; ASTM D638 |
| Flexural Yield Strength | 103 MPa | 14900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 3.44 GPa | 499 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 21.36 J/cm | 40.02 ft-lb/in | ASTM D4812 |
| Tensile Impact Strength | 157 kJ/m² | 74.7 ft-lb/in² | Type S; ASTM D1822 |
| Dart Drop, Total Energy | 101 J | 74.5 ft-lb | ASTM D3029 |
| Taber Abrasion, mg/1000 Cycles | 11 | 11 | CS-17, 1 kg; ASTM D1044 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 146 °C @Thickness 6.40 mm |
295 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 142 °C @Thickness 6.40 mm |
288 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Vicat Softening Point | 154 °C | 309 °F | Rate B/50; ASTM D1525 |
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical without Impact | 130 °C | 266 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 1.52 mm |
V-0 @Thickness 0.0598 in |
UL 94 |
| 5VA @Thickness 3.04 mm |
5VA @Thickness 0.120 in |
UL 94 | |
| Oxygen Index | 36 % | 36 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+17 ohm-cm | >= 1.00e+17 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.05 @Frequency 1.00e+6 Hz |
3.05 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 3.1 @Frequency 50.0 - 60.0 Hz |
3.1 @Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Dielectric Strength | 17.7 kV/mm @Thickness 3.20 mm |
450 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
| Dissipation Factor | 0.00080 @Frequency 50.0 - 60.0 Hz |
0.00080 @Frequency 50.0 - 60.0 Hz |
ASTM D150 |
| 0.0075 @Frequency 1.00e+6 Hz |
0.0075 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
| Hot Wire Ignition, HWI | 60 - 120 sec | 60 - 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | 0.00 - 15 arcs | 0.00 - 15 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | >= 150 mm/min | >= 5.91 in/min | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Radiant Panel Listing | YES | UL Tested |
| Specific Volume | 0.8cm^3/g | ASTM D792 |
| UV-light, water exposure/immersion | F2 | UL 746C |