Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
ASTM D955
PolyOne Maxxam™ PPH-40G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
PolyOne Maxxam™ PPR-40G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Ovation Polymers Opnyl OP66GF43 Nylon 66, Dry as Molded
Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP BX05030 SAN (Europe-Africa-Middle East)
LNP* Lubricomp* BX05030 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
PolyOne Nymax™ GF 600 A 33 Black 28 V Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
PolyOne Therma-Tech™ NJC-6000 TC Nylon 12  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Linear Mold Shrinkage, Flow 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co..
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL HM2300 PP+GF30%
Description: Injection Molding, PP+GF30%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical XG568 MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0020 - 0.0040 in/in

@Thickness 0.125 in
ASTM D955
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity
Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
SABIC Method
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f..
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM 2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Ultem 2313 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region...
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Ultem ATX203R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm

@Time 86400 sec
0.0010 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched
LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics NORYL GFN2V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN2V is a 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco..
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DEP32 PC
LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled
Information from Shinkong Synthetic Fibers Corp.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PX87791 PA 6
LNP* THERMOCOMP* PX87791 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm

@Time 86400 sec
0.0010 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS
LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® VB-8102G MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO DIS 294-4
Wellman Wellamid® GF25-66 XE-N 25% Glass Fiber Reinforced, Engineering Grade Nylon 66
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO DIS 294-4
Wellman Wellamid® MRGF25/15 42H-N1/WE1705-N1 40% Mineral/Glass Fiber Reinforced Nylon 6
Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
on Tensile Bar; E2P method
Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded
Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0025 - 0.0040 cm/cm
0.0025 - 0.0040 in/in
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced
Polyurethane (PUR) based compound. Glass fibers. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Solvay Test
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)  
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..