Material Notes:
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1183
ESCR 100% Igepal® 15 hour

@Temperature 50.0 °C
15 hour

@Temperature 122 °F
ASTM D1693
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.8 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
26 g/10 min

@Load 21.6 kg,
Temperature 190 °C
26 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ISO 306