Indium Corp. Indalloy 199 Gold Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 199 Gold Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 19.08 g/cc
0.6893 lb/in³
Thermal Properties Metric English Comments
Melting Point 360 - 1030 °C
680 - 1890 °F
Solidus 360 °C
680 °F
Liquidus 1030 °C
1890 °F
Component Elements Properties Metric English Comments
Antimony, Sb 0.60 %
0.60 %
Gold, Au 99.4 %
99.4 %