Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay ANTAROX® L 62N Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name ANTAROX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay ANTAROX® L 62N Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: Poloxamer 182CAS: 9003-11-6Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Antarox L-62N is a hydrophilic EO.PO block polymer. Multipurpose emulsifier. Dispersing agent. Suggested for emulsifiable concentrates with polar solvents. Hard Surface Cleaners, Automatic-Dish Washing Detergents, CleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 5.5 - 7.0
5.5 - 7.0
5% Solution; RP-0420
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl Fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear to slightly hazy liquid
RP-0064
Cloud Point 31-33°C
1.0% Solution, RP-0124
Color <150
APHA, RP-0343
Neutralization Number <0.5 mg KOH/mg
pH 7, RP-0343
Copyright © lookpolymers.com All Rights Reserved