Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 GPa | 152 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4215M (EP1X35F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4310M (EP1X30F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4316M (EP1X35AF) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1% Secant; ASTM D790 |
Flint Hills P5M6K-048 Random Copolymer Polypropylene Random copolymer, FDA compliant.Features: Clarified (50 mil plaque haze 10%), antistat, and controlled rheology.Applications: Injection molding: high clarity parts, medical parts, and good organole.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos L40N-00 Polypropylene Impact Copolymer L40N-00 is a nucleated high flow polypropylene, medium impact copolymer for injection molding applications. This resin exhibits an excellent balance of resin flow and mechanical properties. This res.. |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790A |
Ineos R35C-02 Polypropylene Random Copolymer Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antist.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D760-66 |
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.05 GPa | 153 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EF040AE TPO Compound Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB/ML 61 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 805 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | Chord, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7035E5 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Flexural Modulus | 1.05 GPa @Temperature 23.0 °C |
152 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FN718 NC010A Nylon 66 Zytel® FN718 NC010A is a flexible, plasticizer free modified polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, Conditioned Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |