Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4550 VAROX Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4550 VAROX Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
as molded
56
56
post cured- 2 hours at 177°C
57
57
post cured- 4 hours at 204°C
Tensile Strength, Ultimate 9.729 MPa
1411 psi
post cured- 2 hours at 177°C
10.17 MPa
1475 psi
post cured- 4 hours at 204°C
10.91 MPa
1582 psi
as molded
Tensile Strength, Yield 1.55 MPa
225 psi
200%, post cured- 4 hours at 204°C
3.07 MPa
445 psi
at 200%, as molded
3.17 MPa
460 psi
at 200%, post cured- 2 hours at 177°C
Elongation at Break 593 %
593 %
post cured- 2 hours at 177°C
619 %
619 %
post cured- 4 hours at 204°C
693 %
693 %
as molded
Tear Strength 31.2 kN/m
178 pli
post cured- 4 hours at 204°C; Die B
36.3 kN/m
207 pli
as molded; Die B
37.7 kN/m
215 pli
post cured- 2 hours at 177°C; Die B
Copyright © lookpolymers.com All Rights Reserved