Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Tisan Engineering Plastics
Trade Name TISOPLEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow moisture intakeHigh impact resistanceExcellent chemical resistanceElectrical isolationHigh performance/affordable priceEasy processability Mineral filled TISOPLEN compounds have a long lasting thermal-dimensional stability, increased mechanical and hardness characteristics, decreased mold shrinkage and improved surface appearance. Glass fiber reinforcement will impart high tensile strength and impact resistance and yield improvements in thermal characteristics of TISOPLEN products. Excellent resistance to weak acids, weak alkalis, and strong alkalis. Good resistance to strong acids and alcohols. Medium resistance to hydrocarbons and engine fuels. Weak resistance to organic solvents.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
ISO 868
Tensile Strength at Break 26.0 MPa
3770 psi
ISO 527-2
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Break 40 %
40 %
ISO 527-2
Elongation at Yield 38 %
38 %
ISO 527-2
Modulus of Elasticity 1.75 GPa
254 ksi
ISO 527-2
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
Vicat Softening Point 150 °C
302 °F
ISO 306
Heat Distortion Temperature 120 °C
248 °F
ISO 75-2
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
350 V
TS EN 60112
Processing Properties Metric English Comments
Feed Temperature 70.0 °C
158 °F
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Aft-1. Region Temperature
Middle Barrel Temperature 190 - 210 °C
374 - 410 °F
Mid-2. Region Temperature
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Nozzle Temperature 200 °C
392 °F
Melt Temperature 170 - 190 °C
338 - 374 °F
Drying Temperature 80.0 °C
176 °F
Predrying Temperature
Dry Time 1 hour
1 hour
Predrying Time
Moisture Content 0.010 %
0.010 %
ISO 62
Descriptive Properties Value Comments
Block Temperature 45°C