Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Nozzle Temperature = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 200 °C
392 °F
Premix Thermoplastics PRESEAL® TPE 6070
PRESEAL TPE 6070 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sp..
Nozzle Temperature 200 °C
392 °F
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Nozzle Temperature 200 °C
392 °F
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-..
Nozzle Temperature 200 - 274 °C
392 - 525 °F
Average value: 230 °C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer
Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
Nozzle Temperature 200 - 227 °C
392 - 440 °F
Average value: 218 °C Grade Count:65
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Injection
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical AF312C ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible
Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Nozzle Temperature 200 - 240 °C
392 - 464 °F
Injection Molding
LG Chemical KEYFLEX TO1192A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical
Nozzle Temperature 200 - 220 °C
392 - 428 °F
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Extrusion
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical AF360 ABS, TBBA-free Flame Retardant
Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
Nozzle Temperature 200 °C
392 °F
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Nozzle Temperature 200 °C
392 °F
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Nozzle Temperature 200 °C
392 °F
Tisan TISAKRIL® UNR ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 °C
392 °F
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Nozzle Temperature 200 - 210 °C
392 - 410 °F
Injection
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Nozzle Temperature 200 - 270 °C
392 - 518 °F
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Nozzle Temperature 200 - 240 °C
392 - 464 °F
Injection
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 200 - 205 °C
392 - 401 °F
Injection
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Nozzle Temperature 200 - 230 °C
392 - 446 °F
Injection
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Nozzle Temperature 200 - 205 °C
392 - 401 °F
Injection
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..