Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 9007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm | 0.015 - 0.022 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 S Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXFLEX® 810HS TPO
(discontinued **) Description: DEXFLEX® 810HS is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. This material is designed to exceed the requirements .. |
|||
Linear Mold Shrinkage | 0.015 - 0.045 cm/cm @Thickness 3.20 mm |
0.015 - 0.045 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 6042-60A Z Specialty Thermoplastic Elastomer |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D 955 |
RTP Company RTP 800 TFE 10 Z Acetal (POM), PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 HH Nylon 6 for injection molding Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Linear Mold Shrinkage | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
Kolon SPESIN® KP513UG PBT Alloy Resin Extrudable, delusteringApplications: Mono filamentInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Multibase Multi-Flex® D 3804 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
|
Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer Isocorâ„¢ 653 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ 653 is easily processed and has a wide range of applications due .. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | 0.125inch wall |
Spartech EP6220 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1695L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2207 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer 10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.20 mm |
0.015 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company EMI 162 Polypropylene (PP) Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.17 mm |
0.015 - 0.020 in/in @Thickness 0.125 in |
ASTM D 955 |
RTP Company RTP 150 Polypropylene (PP), Flame Retardant - UL94 V-0 RTP 150 is a flame retardant, unreinforced polypropylene material which possesses UL94 flammability and elevated RTI ratings. RTP 150 offers excellent moldability with the living-hinge effect. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.17 mm |
0.015 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 152 LF Polypropylene (PP), Low Flow - Flame Retardant - UL94 V-2 The RTP 152 family of compounds are flame retarded, unreinforced polypropylene materials. They offer excellent moldability, non-corrosive characteristics and the living-hinge effect. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.17 mm |
0.015 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 154 LF Polypropylene (PP), Low Flow - Flame Retardant The RTP 154 family of compounds are flame retarded, unreinforced polypropylene materials. They offer improved physical properties, low specific gravity and excellent moldability vs. traditional V-0.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.20 mm |
0.015 - 0.025 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 200 TFE 10 Z Nylon 6/6 (PA) PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2840 Thermoplastic Elastomer Elastocon® 2840 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2840 is FDA compliant and well suited for cons.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | |
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Ashley Polymers Ashlene® 527LDS-B2 Nylon 66 A high impact lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® GA510 Homopolymer Acetal Resin 10% Glass fiber filled grade with high stiffness and superior dimensional stability.Information provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.17 mm |
0.015 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 2800 B-75A FR Thermoplastic Vulcanizate Elastomer (TPV), Flame Retardant
(discontinued **)< Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.17 mm |
0.015 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 2800B-50D FR Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore D - Flame Retardant 50 Shore D - Flame RetardantComments:50-D DurometerFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pr.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 3.17 mm |
0.015 - 0.025 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1000 TFE 15 Z Polybutylene Terephthalate (PBT), PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 2800B-60A HF Thermoplastic Vulcanizate Elastomer (TPV) 60 Shore A - High Flow
&n 60 Shore A - High FlowComments:60-A DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT.. |