Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 1.75 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.75 GPa
254 ksi
50% RH
Murtfeldt Murylon® 6 Cast Nylon 6
Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia..
Modulus of Elasticity 1.75 GPa
254 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® ESD 7300
PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj..
Modulus of Elasticity 1.75 GPa
254 ksi
Reliance Industries BIOMER P226
compared to PPInformation provided by Reliance Industries
Modulus of Elasticity 1.75 - 3.38 GPa
254 - 490 ksi
Average value: 2.92 GPa Grade Count:79
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 1.75 GPa
254 ksi
ISO 527-2
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Modulus of Elasticity 1.75 GPa
254 ksi
ISO 527
DSM Fibre Intermediates Nyrim® 2025 (Wollastocoat®), Conditioned
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Modulus of Elasticity 1.75 GPa
254 ksi
ISO R527
Arkema Group Orgalloy® LE60 THM Polyamide Alloy
Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Modulus of Elasticity 1.75 GPa

@Temperature 100 °C
254 ksi

@Temperature 212 °F
ISO 527
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
Modulus of Elasticity 1.75 GPa

@Temperature 20.0 °C
254 ksi

@Temperature 68.0 °F
Micropol Isoplas P602 Crosslinkable Polyethylene
Information provided by Micropol Limited
Copyright © lookpolymers.com All Rights Reserved