Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 210 °C | 338 - 410 °F | |
PolyOne OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE) OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2807 HDPE Injection Molding Resin Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Industrial and lubricant pails.Data provided by .. |
|||
Melt Temperature | 170 - 260 °C | 338 - 500 °F | |
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin Features: Excellent balance of stiffness and toughness, low odor.Applications: Margarine and spreads, thin walled containers, frozen food containers.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI LASTIROL R-V0 Polystyrene (PS) (UL94 V-0)
(discontinued **) Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass fiber reinforc.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 222 °C Grade Count:70 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 170 - 210 °C | 338 - 410 °F | Start Point: 190°C |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Melt Temperature | 170 - 210 °C | 338 - 410 °F | Injection Molding |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Melt Temperature | 170 - 240 °C | 338 - 464 °F | Flat film extrusion |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis FA3220 Low Density Polyethylene FA3220 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Unmodified. This grade is developed to give a strong film with balanced shrink properties. Applications FA3220 has bee.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Blown Film Coextrusion |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Melt Temperature | 170 - 215 °C | 338 - 419 °F | |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Melt Temperature | 170 - 230 °C | 338 - 446 °F | Average value: 202 °C Grade Count:18 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Temperature | 170 - 220 °C | 338 - 428 °F | Average value: 200 °C Grade Count:14 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Temperature | 170 - 279 °C | 338 - 534 °F | Average value: 215 °C Grade Count:51 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Melt Temperature | 170 - 260 °C | 338 - 500 °F | |
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin
(discontinued **) Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac.. |
|||
Melt Temperature | 170 - 302 °C | 338 - 576 °F | Average value: 217 °C Grade Count:12 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |