Material Notes:
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Melt Flow 1.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Yield Strength 98.6 MPa
14300 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm,
Temperature -28.9 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature -20.0 °F
ASTM D256
4.27 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
35.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB