Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 950 MPa
138000 psi
Tensile Modulus 70.0 GPa
10200 ksi
Flexural Yield Strength 850 MPa
123000 psi
Flexural Modulus 60.0 GPa
8700 ksi
Compressive Yield Strength 720 MPa
104000 psi
Shear Strength 70.0 MPa
10200 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 60
Tack Life (days) 30