Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 4000 ET-1001 L Polyphthalamide (PPA), Impact Modified - Lubricated |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 800 SI 2 Acetal (POM), Silicone Lubricated |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 899 X 120422 D Acetal (POM), Carbon Nanotube - ESD Protection |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 TL15 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Plaslube® NY-1/TF/13/SI/2 Nylon 66, 13% PTFE, 2% Silicone Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 1000 TFE 10 FR A Polybutylene Terephthalate (PBT), PTFE Lubricated - Flame Retardant |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 200 A TFE 15 Nylon 6 (PA), PTFE Lubricated |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company RTP 200 D MS Nylon 6/12 (PA), Molybdenum Disulfide |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D 790 |
RTP Company EMI 962 Polysulfone (PSU), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Bayshore Vinyl Compounds BRC R409002 Molding Compound BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.Information Provided by Bayshore Vinyl Compounds Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D-790 |
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34 Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and prote.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-15FG-0860 15% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Aaron Industries AAROPRENE® AEN 6600-1 Nylon 6/6 Engineered Resin |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
BASF Capron® B73ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |