Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Techmer ES Plaslube® NY-1/TF/12 Nylon 66, 12% PTFE Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin.. |
|||
Flexural Yield Strength | 98.6 MPa | 14300 psi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS 720 BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |