Polymer Property : Flexural Yield Strength = 14300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 98.6 MPa
14300 psi
ASTM D790
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass
Information provided by Star Plastics, Inc.
Flexural Yield Strength 98.6 MPa
14300 psi
ASTM D790
Techmer ES Plaslube® NY-1/TF/12 Nylon 66, 12% PTFE
Plaslube polytetrafluoroethylene (PTFE) lubricated nylon 66 grades offer the best wear and friction properties of any unreinforced, lubricated nylon compounds, making them ideal materials for bearin..
Flexural Yield Strength 98.6 MPa
14300 psi
ASTM D790
Techmer ES Plastiblend® PC/ABS 720 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.