Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Linear Mold Shrinkage 0.014 - 0.016 cm/cm

@Thickness 3.17 mm
0.014 - 0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80
70 - 80
ASTM D2240
Tensile Strength at Break 4.80 MPa
696 psi
chs 20 in/min; ASTM D412
Elongation at Break 650 %
650 %
chs 20 in/min; ASTM D412
Compression Set 35 %

@Temperature 25.0 °C,
Time 79200 sec
35 %

@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395