PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
15 sec; ASTM D2240
Tensile Strength, Yield 53.4 MPa
7750 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.79 GPa
405 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 88.5 MPa
12800 psi
ASTM D790
Flexural Modulus 2.84 GPa
412 ksi
ASTM D790
Izod Impact, Notched 1.40 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.62 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
5.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
173 J/cm

@Temperature 23.0 °C
0.324 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features High Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Profiles
Users viewing this material also viewed the following: