Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 53.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.1 MPa
7700 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable 3311-xx23D Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength, Yield 53.1 MPa
7700 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 53.1 MPa
7700 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 53.1 MPa
7700 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Tensile Strength, Yield 53.1 MPa
7700 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PCT2000 PC/PCT Alloy
PC/PCT alloy with good balance of physical propertiesAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PCT2010 PC/PCT Alloy, Chemical Resistant
PC/PCT alloy with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Lucent Polymers PC/PBT-1212 Polycarbonate+PBT, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Lucent Polymers PC/PBT-1422 Polycarbonate+PBT, Improved Cold Temp Impact, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Spartech 513 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Spartech 617 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Spartech 829 Static Conductive Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Techmer ES HiFill® PBT 620
Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 2110 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 720 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 830 SS7 BK
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Techmer ES Statiblend® PC/ABS 830 SS7 BK with Stainless Steel Fiber
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM Data
Styron Pulse® 1310 ABS + Polycarbonate
PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM Data
Styron Pulse® 830 ABS + Polycarbonate
PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot..
Tensile Strength, Yield 53.1 MPa

@Thickness 3.20 mm
7700 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM 638
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant
Data provided by Clariant Masterbatches
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Spartech Spectar® UV Copolyester Sheet
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.
Copyright © lookpolymers.com All Rights Reserved