Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 4.27 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy
Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers.
Izod Impact, Notched 4.27 J/cm

@Temperature 23.0 °C
8.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Noble Polymers Regis™ 285107 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Izod Impact, Notched 4.27 J/cm

@Temperature -34.4 °C
8.00 ft-lb/in

@Temperature -30.0 °F
ASTM D256
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified
Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Izod Impact, Notched 4.27 J/cm

@Temperature 22.8 °C
8.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Lucent Polymers PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 4.27 J/cm

@Temperature -30.0 °C
8.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..
Izod Impact, Notched 4.27 J/cm

@Temperature -20.0 °C
8.00 ft-lb/in

@Temperature -4.00 °F
ASTM D 256
MRC Polymers NAXALOYâ„¢ 770-NT137 ABS + PC Alloy
Information provided by MRC Polymers Inc.
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 IM 7050
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® 364 PBT
This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® PC/ABS 720 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® PC/ABS FR 6206
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
8.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PBT IM 1012
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 4.27 J/cm

@Temperature -40.0 °C
8.00 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Valox® 364 PBT
Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 4.27 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
8.00 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
PlastxWorld CEVIAN® S1500 High Heat PC/ABS alloy
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-747R ABS - Extrusion
Attach case and refrigerator
Izod Impact, Notched 4.27 J/cm

@Thickness 6.35 mm
8.00 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Axiall 7450 Rigid PVC, Extrusion
Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res..
Izod Impact, Notched 4.27 - 5.87 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
8.00 - 11.0 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret..
Copyright © lookpolymers.com All Rights Reserved