Material Notes:
PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin has been used in automotive instrument panel and interior trim applications.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Melt Flow 2.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.3 MPa
7010 psi
ASTM Data
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM Data
Elongation at Break 100 %
100 %
ASTM Data
Elongation at Yield 4.8 %
4.8 %
ISO Data
Tensile Modulus 2.10 GPa
305 ksi
ISO Data.
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM Data
5.34 J/cm

@Temperature -50.0 °C
10.0 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 2.40 J/cm²
11.4 ft-lb/in²
ISO Data, Low Temp
6.10 J/cm²
29.0 ft-lb/in²
ISO Data
Impact Test 50.9 J

@Temperature -30.0 °C
37.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
50.9 J

@Temperature 23.0 °C
37.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 113 °C
235 °F
Unannealed; ASTM Data