Material Notes:
Industry Application: RecreationProduct Application: Sports EquipmentDistinct Features: Pigmentable, Low Cost, Good Weatherability, High Molding EfficiencyInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 45
45
ASTM D2583
Hardness, Rockwell M 116
116
ASTM D785
Tensile Strength, Ultimate 48.3 MPa
7000 psi
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
Tangent; ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.40
0.40
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648