Polymer Property : Impact Test = 50.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 50.9 J

@Temperature -30.0 °C
37.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Pulse® B250 ABS + Polycarbonate
PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. ..
Impact Test 50.9 J

@Temperature 23.0 °C
37.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Pulse® B250 ABS + Polycarbonate
PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. ..
Impact Test 50.9 J

@Temperature -30.0 °C
37.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Pulse® 840P ABS + Polycarbonate
PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin..
Impact Test 50.9 J

@Temperature 23.0 °C
37.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Pulse® 840P ABS + Polycarbonate
PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin..
Impact Test 50.9 J

@Temperature -30.0 °C
37.5 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Styron Pulse® EXT 100 ABS + Polycarbonate
PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering ..
Impact Test 50.9 J

@Temperature 23.0 °C
37.5 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Pulse® EXT 100 ABS + Polycarbonate
PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering ..