Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific) High flow PC+ABS. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS (Asia Pacific) AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
0.125in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -40.0 °C |
10.0 ft-lb/in @Temperature -40.0 °F |
0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -18.0 °C |
10.0 ft-lb/in @Temperature -0.400 °F |
ASTM D4812 |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Global PC/ABS-1216 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Global PC/ABS-MC1220 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Haysite H320 Polyester Composite A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective produ.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | Edgewise (LW); ASTM D256 |
Haysite H515 Polyester, High Temp Flex H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | Edgewise (LW); ASTM D256 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Izod Impact, Notched | >= 5.34 J/cm @Temperature 22.8 °C |
>= 10.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7110 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS EP Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | -22°F; ASTM D256 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM Data |
Styron Pulse® 1310 ABS + Polycarbonate PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Asia Pacific) High modulus/impact/heat PPE+PP. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total 50100.1 HDPE blow molding Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging. Blow Molding Stock Temperature 370 – 450 ºF Extrusion melt tempera.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Izod Impact, Notched | >= 5.34 J/cm | >= 10.0 ft-lb/in | ASTM D256 |
Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D648 |
PolyOne Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
(di Information provided by PolyOne™ Corporation |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Izod Impact, Notched | 5.34 - 8.01 J/cm | 10.0 - 15.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |