Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 - 120 °C | 235 - 248 °F | Average value: 117 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D-648 |
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D-648 |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ISO 75Af |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D648 |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 6.40 mm |
235 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP KFB41 (Europe-Africa-Middle East) LNP* THERMOCOMP* KFB41 is a compound based on Acetal Copolymer resin containing Glass Fiber, Glass Bead. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 6.40 mm |
235 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 6.40 mm |
235 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Unannealed; ASTM Data |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® APC100 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D648 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AT-5GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C @Thickness 3.20 mm |
235 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | |
Polimeri Europa KOBLEND PCA 839 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 130°C Main applications fields: a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 113 °C | 235 °F | ASTM D648 |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |