Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin Extem XH2315 Resin |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East) Extem XH2315 Resin |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East) Lexan Copolymer resin with improved chemical resistance, available only in limited colors. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV330 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® 1460, Injection Grade
(discontinued **) Injection molding grade, increased heat and impact resistance, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acqui.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 30YK270 PP SABIC® STAMAX 30YK270 is a 30% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Styrolution NOVODUR® P2MC ABS, Injection Grade Injection molding grade for plating; very good ratio between toughness, heat resistance and flow.Applications: All parts to plating: e.g. sanitary parts. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179-1 |
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by S.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179 |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East) PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels |