Shin-Etsu Silicones KE-3611U Electrically Conductive Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-3611U Electrically Conductive Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ShinEtsu KE3611 U is a black semi conductive silicone compound. It has been designed as a 60 Durometer material with typical volume resistivity values of 5 W cm.Product Features: Suitable for both molding and extrusion.Can be catalyzed with both peroxide and addition cure catalysts.Typical Applications: Key pads.E M I gaskets.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
DBPH Cure
1.16 g/cc
1.16 g/cc
DBPH-50 Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
DBPH Cure
65
65
DBPH-50 Cure
Tensile Strength at Break 4.71 MPa
683 psi
DBPH-50 Cure
4.90 MPa
710 psi
DBPH Cure
Elongation at Break 290 %
290 %
DBPH Cure
320 %
320 %
DBPH-50 Cure
Tear Strength 11.4 kN/m
65.0 pli
Die B; DBPH Cure
11.7 kN/m
67.0 pli
Die B; DBPH-50 Cure
Compression Set 18 %

@Temperature 180 °C,
Time 79200 sec
18 %

@Temperature 356 °F,
Time 22.0 hour
DBPH Cure
Descriptive Properties Value Comments
Cure Agent DBPH
DBPH-50
Cure Type Press Cure