Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 50.9 J @Temperature -30.0 °C |
37.5 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® B250 ABS + Polycarbonate PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. .. |
|||
Impact Test | 50.9 J @Temperature 23.0 °C |
37.5 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® B250 ABS + Polycarbonate PULSE® B250 Engineering resin has been designed to provide a customized balance of low coefficient of linear thermal expansion, low temperature toughness and Class A surface finish paintability. .. |
|||
Impact Test | 50.9 J @Temperature -30.0 °C |
37.5 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Impact Test | 50.9 J @Temperature 23.0 °C |
37.5 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Impact Test | 50.9 J @Temperature -30.0 °C |
37.5 ft-lb @Temperature -22.0 °F |
Instrumented Dart Total Energy |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Impact Test | 50.9 J @Temperature 23.0 °C |
37.5 ft-lb @Temperature 73.4 °F |
Instrumented Dart Total Energy |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |