Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced , Nylon
Manufacturer Styrolution
Trade Name Terblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
dry; ISO 1183
Water Absorption 3.4 %
3.4 %
beginning dry; ISO 62
Moisture Absorption at Equilibrium 1.0 %
1.0 %
beginning dry (23°C/50% R.H.); ISO 62
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 240 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 85.0 MPa
12300 psi
5mm/min; ISO 527
Elongation at Break 3.5 %
3.5 %
5mm/min; ISO 527
Tensile Modulus 6.50 GPa
943 ksi
1mm/min; ISO 527
Flexural Strength 105 MPa
15200 psi
ISO Data
Flexural Modulus 5.50 GPa
798 ksi
ISO Data
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.050

@Frequency 1.00e+6 Hz
0.050

@Frequency 1.00e+6 Hz
IEC 60250
Processing Properties Metric English Comments
Melt Temperature 265 °C
509 °F
Injection molding
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Descriptive Properties Value Comments
Commercial Status Active America
Primary Processing Technique Injection Molding
UL.UL-C Yes