Polyram PlusTek PB890 Nylon 6, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB890 Nylon 6, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
DIN 53479
Water Absorption 8.0 %
8.0 %
DIN 53495
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM-D785
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM-D638
Elongation at Break 100 %
100 %
ASTM-D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM-D790
Izod Impact, Notched 9.00 J/cm

@Temperature 23.0 °C
16.9 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4