Material Notes:
Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. SURLYN® 8528 complies with Food and Drug Administration Regulation 21 CFR 177.1330(a) - - Ionomeric resins, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (c) of the Regulation.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240, ISO 868
Abrasive Hardness 600
600
NBS Index, ASTM D1630
Tensile Strength at Break 29.0 MPa

@Temperature 23.0 °C
4210 psi

@Temperature 73.4 °F
ASTM D638, ISO 527-2
Elongation at Break 450 %

@Temperature 23.0 °C
450 %

@Temperature 73.4 °F
ASTM D638, ISO 527-2
Flexural Modulus 0.220 GPa

@Temperature 23.0 °C
31.9 ksi

@Temperature 73.4 °F
ASTM D790
0.576 GPa

@Temperature -20.0 °C
83.5 ksi

@Temperature -4.00 °F
ASTM D790
Tensile Impact Strength 934 kJ/m²

@Temperature -40.0 °C
445 ft-lb/in²

@Temperature -40.0 °F
ASTM D1822
1160 kJ/m²

@Temperature 23.0 °C
550 ft-lb/in²

@Temperature 73.4 °F
ASTM D1822
Thermal Properties Metric English Comments
Melting Point 66.0 °C
151 °F
Freezing Point; ASTM D3418, ISO 3146
93.0 °C
199 °F
ASTM D3418, ISO 3146
Vicat Softening Point 73.0 °C
163 °F
ASTM D1525, ISO 306
Brittleness Temperature -95.0 °C
-139 °F
ASTM D746
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 6.35 mm
6.0 %

@Thickness 0.250 in
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature <= 285 °C
<= 545 °F
Melt Temperature 185 - 285 °C
365 - 545 °F