Material Notes:
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America and North AmericaMain Properties: ? Dimensional stability, Impact Resistance, Stiffness, and Excellent thermal resistance Applications: TECHNYL C 218 V50 is indicated for pieces that require dimensional stability and good mechanical proprieties like impact at higher temperatures.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO R 527
Elongation at Break 3.0 %
3.0 %
ISO R 527
Tensile Modulus 8.60 GPa
1250 ksi
ISO R 527
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
ISO 180
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
Charpy Impact, Notched 3.40 J/cm²
16.2 ft-lb/in²
ISO 179
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
CEI 93
Dielectric Constant 4.5
4.5
CEI 250
Dielectric Strength 22.0 kV/mm
559 kV/in
CEI 93
Dissipation Factor 0.0090
0.0090
CEI 250
Comparative Tracking Index 475 V
475 V
CEI 112
Users viewing this material also viewed the following: