Polymer Property : Charpy Impact Unnotched = 54.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179/1eU
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179/1eU
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned
Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 50
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 50
Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ?..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50
Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® GVL-6H nat PA*-GF60
Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C140 BK086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding. It has very low warpage.Information provided by Du..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..
Charpy Impact Unnotched 11.5 J/cm²
54.7 ft-lb/in²
ISO 179
BASF Ultramid® 8260 HS PA6 (Dry)
Charpy Impact Unnotched 11.5 J/cm²

@Temperature 23.0 °C
54.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Conditioned, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..