Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 475 V | 475 V | Solution A; IEC 60112 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East) CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended.. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance |
|||
Comparative Tracking Index | 475 V | 475 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Comparative Tracking Index | 475 V | 475 V | Solution A; IEC 60112 |
Solvay TECHNYL® C 216 V45 PA6, 45% glass fiber, DRY Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.Available in: EuropeProduct Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a n.. |
|||
Comparative Tracking Index | 475 V | 475 V | Solution B; IEC 60112 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Comparative Tracking Index | 475 V | 475 V | Solution A; IEC60112 |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Comparative Tracking Index | 475 V | 475 V | CEI 112 |
Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 50 Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ?.. |
|||
Comparative Tracking Index | 475 V | 475 V | CEI 112 |
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 50 Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:.. |
|||
Comparative Tracking Index | 475 V | 475 V | Solution B; IEC 60112 |
Solvay TECHNYL® C 50 H2 PA6, DRY Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p.. |
|||
Comparative Tracking Index | 475 V | 475 V | ASTM D3638 |
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Unitika M1030DH PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Comparative Tracking Index | 475 V | 475 V | dry; IEC 60112 |
DSM Novamid® 1013G30 1 NA PA6-GF30 30% Glass Reinforced, Injection Molding |
|||
Comparative Tracking Index | 475 V | 475 V | dry; IEC 60112 |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® TSS/4 LF 2 PA666 Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import.. |
|||
Comparative Tracking Index | 475 V | 475 V | DAM; IEC 60112 |
DuPont Performance Polymers Minlon® 22C BK086 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance.. |
|||
Comparative Tracking Index | 475 V | 475 V | conditioned; IEC 60112 |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 475 V | 475 V | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 475 V | 475 V | Test solution A; IEC 112 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Comparative Tracking Index | 475 V | 475 V | IEC 60112 |
Lanxess Durethan® BKV 35 H2.0 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: automotive structures |
|||
Comparative Tracking Index | 475 V | 475 V | A solution |
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |