Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.0 kV/mm | 559 kV/in | dry; IEC 60243-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ISO.243 DIN.53481 |
Omnia Plastica Akulon® PA 66.6 Akulon GX - Dry Copolymer of nylon with excellent mechanical features, it combines the good impact resistances of PA6 as well as the higher stiffness of PA66. For this reason it machines very well on automatic tool.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ASTM D149 |
Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | |
Momentive Performance Materials TSE326 Red Adhesive Sealant, Non-Corrosive Flowable High Temperature One-part heat cure. Typical uses: Assembly and gasketing.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | |
Momentive Performance Materials TSE3941 Flame Retardant Adhesive Sealant, White TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ASTM D149/DIN 53481 |
Kolon KOPA® KN163G30 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | IEC 243-1 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | IEC 60243 |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | IEC 60243 |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, Conditioned Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | JIS K2111 |
Toyobo PELPRENE™ P95C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo T-750 Nylon, Painting Grade Key Feature: Glass fiber and mineral reinforced, high heat distortion gradesInformation provided by Toyobo Co., Ltd |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | IEC 60243-1 |
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSG-50/4 PA666-GF50 Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High sti.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | Short time; ASTM D149 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
ASTM D149 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® 301-G10F PBT Resin 10% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® 3030 PET Resin High mechanical strength, Creep resistant, Low frictionInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 3.20 mm |
559 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | ASTM D149/DIN 53481 |
Kolon Kopa® KN153G15 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Dielectric Strength | 22.0 kV/mm | 559 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROLYTE Polyethylene terephthalate This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance. Applications include pump components, coil bodies, ball bearing cups and prote.. |