Mechanical Properties Metric English Comments
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol..
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)
This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch..
Tensile Modulus 8.60 GPa
1250 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527-1,-2
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibersInformation provided by LANXESS.
Tensile Modulus 8.60 GPa
1250 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527-1,-2
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Modulus 8.60 GPa
1250 ksi
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 8.60 GPa
1250 ksi
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 8.60 GPa
1250 ksi
ISO R 527
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 50
Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon DE002E PC (Europe-Africa-Middle East)
LNP* STATKON* DE002E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features include; Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEL329EP PC (Europe-Africa-Middle East)
LNP* STATKON* DEL329EP is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features include: Electrically Conductive, Internally Lubricated, Flame retard..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66
LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 8.60 GPa
1250 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific)
PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump ..
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding.
Tensile Modulus 8.60 GPa
1250 ksi
1 mm/min; ISO 527-1
Sax Polymers SAXAMID 226F5 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has high mechanical strength in combination with good flow properties.Information provid..
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Plenco 2000 Phenolic, Granular, Compression Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Plenco 2308 Phenolic, Granular, Injection Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced
Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram.
Tensile Modulus 8.60 GPa
1250 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
Tensile Modulus 8.60 GPa
1250 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Tensile Modulus 8.60 GPa
1250 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Tensile Modulus 8.60 GPa
1250 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Copyright © lookpolymers.com All Rights Reserved