Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
RTP Company RTP 4507 Aliphatic Polyketone, Glass Fiber 40%  (discontinued **)
Properties and average values of injection molded specimens; data provided by RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC
LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC
LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated.
Density 1.56 - 1.60 g/cc
0.0564 - 0.0578 lb/in³
ISO R 1184
Fainplast Compounds RK 335/1 Rigid PVC, Extrusion Lead Free
Profiles
Density 1.56 g/cc
0.0564 lb/in³
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183/A
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: ..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP DF0079 PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF0079 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer
LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Techmer ES HiFill® PET GF30 X 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Density 1.56 g/cc
0.0564 lb/in³
Laminate
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form
Fiber: IM7-12KInformation provided by HexCel
Density 1.56 g/cc
0.0564 lb/in³
(DAM); ISO 1183
DSM Akulon® K224-G0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50
Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45
Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
EMS-Grivory Grivory® TSG-50 PA666-GF50
Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne..
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Ensinger Tecapeek® XP-91BHT Compression Molded PEEK HT Compound, 30% Fiberglass, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based ..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM
GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Density 1.56 g/cc
0.0564 lb/in³
Side 1 Silicone Property; Arlon SQA-TMS-024
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
BASF Petra® 7010 WT 7729 15% Glass Filled PET
Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface ..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET
Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Conditioned)
Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu..
Density 1.56 g/cc
0.0564 lb/in³
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Celanese Celstran® PA66-GF50-02-US Nylon 66, 50% Glass Reinforced
50 % Long glass fiber reinforced, heat stabilized, Nylon 6/6Information provided by Celanese
Density 1.56 g/cc

@Temperature 23.0 °C
0.0564 lb/in³

@Temperature 73.4 °F
ASTM D792
Beijing Ranger Chem PBT-201-G25 291 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Density 1.56 g/cc
0.0564 lb/in³
(DAM); ISO 1183
DSM Akulon® K-FHG0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792