Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 50 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 50 Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ?.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179/1eA |
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Charpy Impact, Notched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179/1eA |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |