Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent combination between thermal and mechanical properties.Available in: Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: It is used in a wide variety of industries.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183/A
Water Absorption 0.78 %

@Temperature 23.0 °C,
Time 86400 sec
0.78 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0062 cm/cm
0.0062 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ISO 527 Type 1A
Elongation at Break 3.6 %
3.6 %
ISO 527 Type 1A
Tensile Modulus 10.5 GPa
1520 ksi
ISO 527 Type 1A
Flexural Strength 290 MPa
42100 psi
ISO 178
Flexural Modulus 8.80 GPa
1280 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 95.0 kJ/m²
45.2 ft-lb/in²
ISO 180/1U
Charpy Impact Unnotched 8.90 J/cm²
42.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 255 °C
491 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Oxygen Index 23 %
23 %
ISO 4589
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
ISO 60695-2-12
650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
Ignition Temperature; ISO 60695-2-13
750 °C

@Thickness 1.60 mm
1380 °F

@Thickness 0.0630 in
ISO 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 6.00e+14 ohm
6.00e+14 ohm
IEC 60093
Dielectric Constant 3.75
3.75
IEC 60250
Dielectric Strength 40.0 kV/mm
1020 kV/in
IEC 60243
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 500 V
500 V
Solution B; IEC 60112
600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C
Copyright © lookpolymers.com All Rights Reserved