Polymer Property : CTE, linear, Parallel to Flow = 25.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East)
LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 150 °C
13.9 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific)
LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS
LNP STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East)
LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East)
Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66
LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is ..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X640 Resole Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bakelite Group
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X680 Novolac Phenolic
Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X689 Novolac Phenolic
Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop..
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30
Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate..
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BG-25 S PA6-GF25
Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi..
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BG-35 S PA6-GF35
Information provided by EMS Grivory
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TC155 PA46 FR(17)
Thermal conductive material, Flame Retardant, Heat Stabilized
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
DSM Arnite® AV2 370 XL PET-GF35
35% Glass Reinforced, Low Outgassing
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-1/-2
DSM Arnite® AV2 370 XT PET-GF35
35% Glass Reinforced, Applications with extremely narrow tolerances
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-2
Celanese CELANEX 1462Z PBT, 30% Glass Reinforced
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-2
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-2
Celanese CELANEX 3300-2FC PBT, 30% Glass Reinforced
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
ISO 11359-2
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.Information provided by Celanese
CTE, linear, Parallel to Flow 25.0 - 35.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
13.9 - 19.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 20.0 °C
13.9 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate
Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.Information provided by Vyncolit, a Sumitomo Bakelite Group
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TC502 PA46