Material Notes:
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material for casual, sport and protective foot wear. The features offered include:DurabilityExcellent surface definitionAbrasion resistanceSlip resistancePhthalate free TPU Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ISO 868
Tensile Strength at Break 24.0 MPa
3480 psi
ISO 37
Elongation at Break 600 %
600 %
ISO 37
100% Modulus 0.00400 GPa
0.580 ksi
ISO 37
300% Modulus 0.00700 GPa
1.02 ksi
ISO 37
Tear Strength 70.0 kN/m
399 pli
ISO 34B
Abrasion 35
35
mm<sup>3</sup>; ISO 4649
Compression Set 20 %
20 %
ISO 815
Processing Properties Metric English Comments
Feed Temperature 25.0 - 35.0 °C
77.0 - 95.0 °F
Rear Barrel Temperature 175 - 185 °C
347 - 365 °F
Middle Barrel Temperature 180 - 190 °C
356 - 374 °F
Front Barrel Temperature 185 - 195 °C
365 - 383 °F
Nozzle Temperature 175 - 190 °C
347 - 374 °F
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa
290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Screw Speed 20 - 80 rpm
20 - 80 rpm
Descriptive Properties Value Comments
Compression Ratio 2-3:1
L/D Ratio 20-25:1
Ross Flex -10°C, BS 5131