Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GF 30 HI PA66, 30% glass fibre, improved strength FeaturesPA 66 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength .. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | STN EN 60243-2 |
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Kazanorgsintez 102-16 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Dielectric Strength | >= 40.0 kV/mm @Frequency 50.0 Hz |
>= 1020 kV/in @Frequency 50.0 Hz |
For cable masterbatches, at alternating voltage frequency |
Kazanorgsintez P2KP Polyethylene Pigment Masterbatches Production Method: P2KP polyethylene pigment masterbatches are produced on the basis of low density polyethylene with high content of masterbatches. Application: P2KP polyethylene pigment masterbatc.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Ineos ABS Triax® 1315 GF ABS + Polyamide Blend (DAM) Key Features:Contains FillerSuitable processing methods:Injection molding |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | VDE 0303/4 |
Polyram RamShine PW300G7 SAN, 35% Glass Fiber 35% glass fiber reinforced SAN for very high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-30 FC PA6-GF30 Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface .. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GVZ 45 HWCP 45% Glass Fiber Nylon 6, Impact Resistant, Good Surface Finish, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | No thickness given |
ConocoPhillips Hydroclear® 68 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform N 2640 Z2 UNC Q600 POM Ultraform N2640 Z2 UNC Q600 is an elastomer-modified grade of POM for injection molding with high impact strength. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15 Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |