Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Feed Temperature | 265 - 270 °C | 509 - 518 °F | |
Solvay TECHNYL® eXten D247 F Nylon 66 & 610 Description: Polyamid 66 & 610, impact modified, alkali resistance, mold release, for injection molding. This material is available in natural color and in colors on requestAvailable in: Asia Pacifi.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Feed Temperature | 265 - 270 °C | 509 - 518 °F | |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Feed Temperature | 265 - 270 °C | 509 - 518 °F | |
Solvay TECHNYL® 27010ST PA66, DRY Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of.. |
|||
Feed Temperature | 265 - 270 °C | 509 - 518 °F | |
Solvay TECHNYL® 2710IR PA66, DRY Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Feed Temperature | 265 - 285 °C | 509 - 545 °F | |
Solvay TECHNYL® A 208KBK-10N-L PA66, DRY Description: Polyamide 66, highly UV-resistance, toughness modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL A 208K BK 10N-L is used in all sectors of industry, .. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:.. |
|||
Feed Temperature | 265 - 275 °C | 509 - 527 °F | |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |