Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. Testing conducted on samples dry as molded and samples conditioned to 50% relative humidity in accordance with ISO-1110, Accelerated Method.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Heat Resistance; High Stiffness; High Strength; High Temperature Strength; Low Moisture AbsorptionUses: Automotive Applications; Automotive Electronics; Automotive Interior Parts; Automotive Under the Hood; Cell Phones; Connectors; Fuel Lines; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Power/Other ToolsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications 3M 11-0003-5762-1 X62 4200; ASTM D4000 PA121 G35 Color: BK324 Black; ASTM D4000 PA121 G35 Color: NT Natural; ASTM D6779 PA121G35; BOSCH N28 BN05-OX1 BN0510-GF35-0Anf01SO Color: NT Natural; BOSCH N28 BN05-OX1 BN0510-GF35-0Asw01SO Color: BK-324 Black; CHRYSLER MS-DB-478 CPN4242 Color: NT Natural; CHRYSLER MS-DB-478 Type A CPN3598 Color: BK324 Black; DELPHI M-53290 Color: BK324 Black; DELPHI M-53290 Color: NT Natural; DELPHI M-6071 Color: NT Natural; DELPHI MS-5216 Color: BK324 Black; DELPHI MS-5216 Color: NT Natural; FORD WSP-M4D843-A Color: BK324 Black; FORD WSP-M4D843-A Color: NT Natural; GM GMP.PPA.004 Color: BK324 Black; GM GMP.PPA.004 Color: NT Natural; GM GMW15702-110020 >PPA+GF33< (A4, A22, A64, BA633, DC1473, G20, KM1158, KS2300, LS20, RS9, SS260, Z1) Color: NT Natural; GM GMW16356P-PPA-GF35 Color: BK-324 Black; GM GMW16356P-PPA-GF35 Color: NT Natural; IMDS ID 21195756 Color: Black; IMDS ID 21195756 Color: Natural; TRW S-13318701 Color: BK543 Black; VALEO VMS-4470 Color: BK324 Black; VALEO VMS-4470 Color: NT Natural; YAZAKI YPES-25-02-135 Color: Colors; YAZAKI YPES-25-02-135 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Dry; ISO 1183
Filler Content 33 %
33 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 193 MPa
28000 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 13.1 GPa
1900 ksi
ASTM D638
Flexural Strength 254 MPa
36800 psi
ASTM D790
Flexural Modulus 11.4 GPa
1650 ksi
ASTM D790
Shear Strength 88.9 MPa
12900 psi
ASTM D732
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 313 °C
595 °F
Dry; ISO 11357-3
313 °C
595 °F
Dry; DSC
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
ASTM D257
Dielectric Constant 4.3

@Frequency 1.00e+6 Hz
4.3

@Frequency 1.00e+6 Hz
ASTM D150
4.7

@Frequency 60.0 Hz
4.7

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 21.0 kV/mm

@Thickness 3.20 mm
533 kV/in

@Thickness 0.126 in
ASTM D149
Dissipation Factor 0.0090

@Frequency 60.0 Hz
0.0090

@Frequency 60.0 Hz
ASTM D150
0.022

@Frequency 1.00e+6 Hz
0.022

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 550 V
550 V
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Part Marking Code >PA6T/6I/66-GF33<
ISO 11469
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
UL File Number E95746 (Global)