Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.48 g/cc | 0.0535 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 6 GF 15 T 25 Polyamide 6, 15% Glass Fiber, 25% Micronized Talc FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form / no screw after co.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D221 Q25 PBT, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Nilit FRIANYL C73 MG40 Nylon 6.6/6 for injection molding, 40% mineral filled Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | 9741A |
Lord Adhesives Aeroglaze® 9741 Epoxy Primer/Tie-Coat Aeroglaze® 9741 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9741 primer/tie-coat is applied to scuff-sanded urethane top coats and e.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific) LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF/M40 HS L BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackProc.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF/M40 IG BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessing Method: In.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific) LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific) LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008 |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP RX05494 PA 66 LNP* Thermocomp* RX05494 is a compound based on Nylon 6/6 resin containing glass fiber fillers. Added features of this material include: Heat Stabilized. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | DIN 53479 |
Polyram PA310G8 Nylon 66, 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC415 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 339 Polyester Film, 380 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | Cured |
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
DuPont Teijin Films Melinex® WLB Polyester Film, 500 Gauge Melinex® WLB is a polyester film with a white surface, a light grey surface and very high opacity. General Product Info: Melinex® WLB offers a film with a white surface and very high opacity. It c.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |