Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI) Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)
(discontinued **) Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |