Polymer Property : Izod Impact, Notched = 0.590 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Plaskolite Optix® CA-1000 I Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
NYCOA 534 H High Viscosity, Heat Stabilized Nylon 6 Resin
NYCOA 534 H is a high viscosity; heat stabilized, nucleated Nylon 6 resin. The high viscosity and fast set-up time make an excellent material for extrusion of tubing, rods, sheet and film. Because o..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6)
The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer)
Information provided by PolyOne
Izod Impact, Notched 0.590 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Izod Impact, Notched 0.590 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ GF 1200 A 13 HS Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Izod Impact, Notched 0.590 J/cm

@Temperature -40.0 °C
1.11 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Rotuba H2 Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Asahi Kasei Tenac® FA405 Acetal Homopolymer, Low Friction Grade  (discontinued **)
Contains fluoropolymer and lubricant; excellent friction and wear on plastics.Applications: Bearings for printers, cams, gears.This product is not a part of the standard product line dated 2003.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose  (discontinued **)
General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Asahi Kasei Tenac®-C 7510 Acetal Copolymer, High Flow  (discontinued **)
High-flow grade, suited for thin-wall, long-flow-distance moldings.Applications: Lighters, aerosol bottles, fasteners.This product is not a part of the standard product line dated 2003.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Kolon Kopa® KN1331 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Kolon Kopa® KN138R Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
SABIC Innovative Plastics ULTEM CRS5011R PEI
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.590 J/cm

@Thickness 3.17 mm
1.11 ft-lb/in

@Thickness 0.125 in
ASTM D256
Entec Hypro™ PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced
Information provided by Entec
Izod Impact, Notched 0.590 J/cm

@Thickness 3.17 mm
1.11 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-1001 TF20 20% Talc Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66
Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 119 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 830L Nylon 6
Basic Nylon 6, medium viscosity, lubricated.Data provided by the manufacturer
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 830LB Nylon 6
Basic Nylon 6, medium viscosity, lubricated black.Data provided by the manufacturer
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resi..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 830LW Nylon 6
Basic Nylon 6, medium viscosity, lubricated for general purpose injection molding.Data provided by the manufacturer
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® RH180 Acetal
Extrusion grade reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. Available in Natural and Black. Natural is designated RH180; Black is designated RH180B.Data provid..
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® RH190H Acetal
General purpose reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated RH190H-..
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® R190H Acetal
General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3..
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® VSR4150 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.