Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPC-20T Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 Zip 0 Black 13 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | 0.125 in.; ASTM D256 |
Resirene Resirene® 2220 Medium Impact Polystyrene Features:High FlowEasy ProcessingGood GlossHigh Tensile ModulusFDA Rating: 21 CFR 177.1640High ProductivityExternal LubricatedApplications:InjectionThin Wall ApplicationsHard to Fill MoldsHangersVid.. |
|||
Izod Impact, Notched | 0.590 - 1.17 J/cm | 1.11 - 2.20 ft-lb/in | Average value: 0.950 J/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® FA405 Acetal Homopolymer, Low Friction Grade
(discontinued **) Contains fluoropolymer and lubricant; excellent friction and wear on plastics.Applications: Bearings for printers, cams, gears.This product is not a part of the standard product line dated 2003. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® LA531 Acetal Homopolymer, High Lubricity
(discontinued **) High-lubricity block copolymer with excellent friction and wear characteristics, especially on POM.Applications: Gears, keyboard parts.This product is not a part of the standard product line dated 2.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Kolon Kopa® KN1331 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Kolon Kopa® KN138R Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm |
1.11 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature 23.0 °C |
1.11 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® VAC3003 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -40.0 °C |
1.11 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 830L Nylon 6 Basic Nylon 6, medium viscosity, lubricated.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | |
UBE UBEPOL BR15HB HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR15HB is characterized by the highest branching of these 3 grades and is adapted by many PS manufacturers.Information provided by UBE. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 830LW Nylon 6 Basic Nylon 6, medium viscosity, lubricated for general purpose injection molding.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Kolon Kopa® KN173MS Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R190H Acetal General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH
(di AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |
|||
Izod Impact, Notched | 0.590 J/cm @Diameter 3.17 mm |
1.11 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |