Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon PAI has the h.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4630 Polyamide-imide (PAI) Torlon® 4630 is an injection-moldable, wear-resistant grade of polyamide-imide (PAI), that has been formulated to give outstanding wear resistance in non-lubricated applications. Torlon® PAI h.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Rear Barrel Temperature | 304 °C | 579 °F | |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)
(discontinued **) Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Rear Barrel Temperature | 304 - 318 °C | 579 - 604 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |